ABS Granules Grade Selection Guide: High-Impact, High-Flow, High-Gloss & Heat-Resistant ABS for Appliances, Automotive & Consumer Products
ABS (Acrylonitrile Butadiene Styrene) is one of the most widely used plastics in India. It is in mixer-grinder bodies, two-wheeler panels, switch plates, TV back covers, helmets, luggage, and toys. But "ABS" is not one material. It is a family of grades, and picking the wrong one is one of the most common reasons for cracked parts, poor gloss, or warped housings.
At Jay Plast, we stock natural and pre-coloured ABS granules from leading producers including ABSOLAC, TAITALAC, and POLIMAXX. In this guide, we explain the main ABS grade types, how to match them to your product, and how to mould ABS without common defects.
1. What Each Part of ABS Does
ABS is made from three building blocks. Changing their balance changes the grade:
- Acrylonitrile (A): Adds chemical resistance, heat resistance, and surface hardness.
- Butadiene (B): A rubber that adds toughness and impact strength, especially at low temperatures.
- Styrene (S): Adds gloss, rigidity, and easy flow during moulding.
More butadiene gives a tougher but less glossy grade. More styrene gives a shinier, easier-flowing grade with lower impact strength. Every ABS grade is a balance of these three.
2. The Main ABS Grade Types
| Grade Type | Typical MFI (220°C / 10 kg) | Notched Izod Impact | Heat Deflection (1.8 MPa, annealed) | Typical Uses |
|---|---|---|---|---|
| General Purpose | 18–25 g/10 min | 180–250 J/m | 85°C–95°C | Appliance housings, switch boxes, toys |
| High Impact | 5–15 g/10 min | 300–450 J/m | 85°C–95°C | Helmets, luggage, two-wheeler panels |
| High Flow | 35–60 g/10 min | 120–200 J/m | 80°C–90°C | Thin-wall parts, large TV covers, multi-cavity tools |
| High Gloss | 15–30 g/10 min | 150–220 J/m | 85°C–95°C | Kitchen appliances, cosmetic parts, visible panels |
| Heat Resistant | 5–15 g/10 min | 150–250 J/m | 100°C–110°C | Hair dryers, car interior parts near heat sources |
| Electroplating Grade | 10–25 g/10 min | 200–300 J/m | 90°C–100°C | Chrome bathroom fittings, car badges and trims |
| Flame Retardant (FR) | 20–45 g/10 min | 100–200 J/m | 75°C–85°C | Electrical enclosures, adapters, chargers |
These are typical industry ranges. Always check the technical data sheet for the exact grade.
3. How to Choose the Right ABS Grade
Ask these five questions about your part:
1. Will it be dropped or hit?
If the part must survive drops, knocks, or cold weather (helmets, luggage, outdoor parts), choose a high-impact grade.
2. Is the wall thin or the flow path long?
Large, thin parts like TV back covers or air cooler bodies need a high-flow grade to fill the mould fully without short shots or high pressure.
3. Will customers see and touch it?
Visible appliance surfaces need a high-gloss grade with a polished, warm mould for a scratch-free, shiny finish.
4. Will it get hot?
Parts close to motors, heaters, or car dashboards in the summer sun need a heat-resistant grade so they do not warp. If you need even higher heat or impact, consider PC+ABS blends.
5. Does it need to carry electricity or pass a fire test?
Electrical enclosures that must meet UL94 V-0 or similar standards need an FR grade.
4. Natural vs. Pre-Coloured ABS
Moulders can colour ABS in two ways:
- Natural ABS + masterbatch: Flexible, good for short runs and many colours. But dosing errors and poor mixing can cause colour streaks and batch-to-batch variation.
- Pre-coloured ABS compound: The colour is already compounded into every granule. This gives consistent colour from batch to batch, no dosing equipment, and fewer rejected parts.
Jay Plast stocks ABS in popular ready colours, including jet black, white, red, light grey, blue, and green, as well as natural grades for your own masterbatch.
5. Processing Guide: Moulding ABS Without Defects
1. Drying
ABS absorbs moisture from the air, especially in the Indian monsoon:
- Drying Temperature: 80°C–85°C for 2 to 4 hours.
- Target Moisture: Below 0.1% (below 0.05% for electroplating and high-gloss parts).
2. Temperature Settings
- Melt Temperature: 210°C–250°C (up to 260°C for high-flow, thin-wall parts).
- Mould Temperature: 40°C–80°C. Use the higher end for high-gloss and electroplating parts.
- Avoid melt temperatures above 270°C. Overheated ABS can yellow and lose impact strength.
3. Common ABS Defects and Fixes
| Defect | Likely Cause | Fix |
|---|---|---|
| Silver streaks | Wet material | Dry properly before moulding |
| Flow marks / tiger stripes | Mould too cold, slow injection | Raise mould temperature, increase speed |
| Weld lines | Two flow fronts meeting cold | Raise melt and mould temperature, move gate, add venting |
| Peeling / layering (delamination) | Contamination with PP, PE or other plastics | Clean hopper and barrel, check regrind source |
| Cracks near screws | High moulded-in stress | Use a warmer mould, reduce packing pressure |
| Low gloss | Mould too cold or not polished | Raise mould temperature, polish tool |
6. Virgin vs. Reprocessed ABS
For visible parts, electroplating, and safety parts like helmets, virgin ABS is the right choice. For hidden brackets, internal covers, and non-critical parts, good-quality reprocessed ABS can reduce material cost significantly. Read our guide on reprocessed vs. virgin plastics for more on this trade-off.
7. Buy ABS Granules from Jay Plast
At Jay Plast, we supply:
- Virgin ABS from ABSOLAC, TAITALAC, POLIMAXX, and other leading producers.
- Pre-coloured ABS in black, white, red, grey, blue, green, and more.
- PC+ABS blends for parts that need extra heat and impact resistance.
- Grade selection support from our technical team.
Based in Mumbai, we supply appliance makers, auto component manufacturers, and injection moulders across Maharashtra, Gujarat, Delhi NCR, Tamil Nadu, Karnataka, and all of India.
Contact Jay Plast today for ABS grade recommendations, data sheets, samples, and competitive per-kg pricing!