How Much Regrind Can You Use in Injection Moulding? Safe Regrind Limits for PP, ABS, PC, Nylon, POM, PBT & Glass-Filled Grades

Every injection moulding shop produces waste: runners, sprues, start-up parts, and rejects. Grinding this scrap and feeding it back into the machine, known as regrind, is one of the easiest ways to cut material costs. But too much regrind, or badly handled regrind, can cause brittle parts, colour changes, black specks, and failed customer tests.

So how much regrind is safe? The honest answer is: it depends on the material, the part, and how well you manage the regrind. At Jay Plast, we supply both virgin and reprocessed engineering plastics, and we help moulders get the balance right. This guide explains typical regrind limits for common plastics and the best practices that keep quality steady.


1. What Happens to Plastic Each Time It Is Remelted

Every time plastic is melted, sheared in the screw, and cooled, it is slightly damaged:

  • Polymer chains get shorter, which lowers toughness and impact strength.
  • Melt flow increases (higher MFI), because shorter chains flow more easily.
  • Colour can shift, often towards yellow.
  • Glass fibres break into shorter pieces, which reduces strength and stiffness in glass-filled grades.
  • Additives get used up, including heat stabilisers, UV stabilisers, and flame retardants.

The more sensitive the plastic, and the more times it has been melted, the bigger the effect.


2. Typical Regrind Limits by Material

MaterialTypical Regrind LimitMain Watch-Outs
PP, PE25%–50% (more for non-critical parts)Very tolerant. Watch colour and MFI drift.
ABS20%–30%Yellowing, loss of impact strength, gloss changes
SAN20%–25%Clarity loss, black specks
Polycarbonate (PC)15%–25%Must be dried. Very sensitive to moisture and overheating.
PC+ABS15%–25%Impact loss, especially at low temperatures
Nylon PA6 / PA6620%–25%Must be dried. Yellowing, brittleness
Glass-Filled Grades (GF30 etc.)15%–25%Fibre breakage lowers strength
POM (Delrin / Acetal)20%–25%Degraded POM gives off formaldehyde. Never use burnt or discoloured regrind.
PBT20%–25%Must be dried. Hydrolysis lowers toughness.
Flame-Retardant (FR) Grades10%–20%Flame rating may be lost. Re-test parts.
PPS, PSU, PPSU20%–25%Generally stable, but must be dried and kept clean
Medical, optical, or safety-critical partsOften 0%Customer approval and testing required

These are typical industry ranges. Your customer's specification and your own part testing always come first.


3. Why a Steady Regrind Ratio Matters

Some moulders worry that regrind gets melted again and again forever. In practice, at a constant ratio, very little material is melted many times.

For example, at a steady 25% regrind ratio:

  • About 75% of the material in each shot is melting for the first time.
  • Only about 6% has been melted twice or more before.
  • Less than 2% has been melted three or more times before.

The real problems come from uneven ratios, for example running 10% one hour and 60% the next because a big bin of rejects was dumped into the hopper. This makes melt flow, colour, and strength change from shot to shot.

Use a proportioning blender or loader to keep the ratio steady.


4. Regrind Best Practices

1. Keep It Clean and Separate

  • Store regrind by material, grade, and colour. Mixing ABS with PC, or nylon with POM, causes peeling, brittleness, or even dangerous gas release.
  • Keep regrind bins covered to stop dust, oil, and floor dirt getting in.
  • Never regrind parts that were burnt, degraded, or contaminated.

2. Grind It Right

  • Use sharp granulator blades. Blunt blades create dust and fines that burn in the barrel and cause black specks.
  • Screen out fines and dust before use.
  • Aim for a regrind size close to the size of virgin granules, so it feeds and melts evenly.

3. Dry It

  • Regrind of hygroscopic plastics (PC, nylon, PBT, PC+ABS, ABS, TPU) must be dried just like virgin material, often for slightly longer.
  • Regrind left in open bins in the monsoon can be wetter than virgin granules.

4. Grind Close to the Machine

  • Beside-the-press granulators that feed runners straight back into the hopper keep regrind fresh, dry, and uncontaminated.

5. Test Regularly

  • MFI test: Compare regrind blends with virgin material. A rise of more than 20%–30% in MFI often signals too much degradation.
  • Impact or drop tests on finished parts.
  • Colour checks against a master sample.
  • For FR parts, re-test the flame rating when you change the regrind ratio.

5. Regrind vs. Reprocessed Granules

If your own scrap is not enough, or you want to save more on hidden or non-critical parts, reprocessed granules are another option. These are scrap plastics that have been cleaned, sorted, re-compounded, and pelletised under controlled conditions. Good-quality reprocessed granules have more consistent properties than mixed in-house regrind. Read our guide on reprocessed vs. virgin plastics to learn more.


6. Get Virgin and Reprocessed Granules from Jay Plast

At Jay Plast, we supply:

  • Virgin engineering plastics: ABS, PC, PC+ABS, SAN, nylon, PBT, POM, PPS, PSU, PPSU, and TPU.
  • High-grade reprocessed granules for cost-saving applications.
  • Technical advice on regrind ratios and blending.

We serve injection moulders in Mumbai, Pune, Gujarat, Delhi NCR, Chennai, Bangalore, and across India.

Contact Jay Plast today to find the right mix of virgin and reprocessed material for your parts!